Prepare the seam

Surfaces must be clean and dry. Overlap is typically 100 mm. Trial welds are made at the start of each shift and checked for peel strength before production welding begins.

Control temperature and speed

Welder temperature, speed and roller pressure are set by the resin and sheet thickness. Too hot or too slow produces brittle seams; too cold leaves unbonded areas that leak under head.

T-joints, penetrations and seam testing

T-joints and pipe boots are the most common leak paths. They should be reinforced with extrusion welding or a patch, not left as a simple overlap. Air testing (or vacuum testing for extracted seams) is performed on every weld. Results are recorded by seam number, and the record forms part of the handover dossier.

Basis and limits. This note is based on GB/T 17643-2011, GB/T 17642-2008, GB/T 17638-2017 and GB/T 18173.1, together with Hengyang batch test practice. It is general technical guidance, not a design for a specific project. Confirm thickness, layer build-up, welding parameters and acceptance criteria against the project drawing and specification.

Related products

Need a project-specific answer?

Send the drawing and design head. We will check the proposed thickness, cushion and weld detail against the specification.

Ask an engineer

Send your project parameters, get a material schedule and quote

Drawings, head, area and chemical exposure are enough for a first selection. We reply within one working day.

Call +86 400-150-1689 Send project details
Call sales WhatsApp Get quote Products